Wear parts insert TIC material, 2-4 times lifetime, highly recommended!

Liners

Liners (including side liners and main liners) are available for almost any machine, and forged from standard manganese steel or low alloy steel.

Austenitic manganese steel:

Chemical compositionC (Max)MnSiCrPS
 1.05-1.2011.00-19.00≤1.001.50-2.50≤0.06≤0.10
Mechanical properties

 

UTS (KSI)YS (KSI)EL%Hardness(BHN)Charpy V-notch(room temp)
90-140 50-7024-40200-25090-160 ft.lb

Low Alloy steel:

Chemical compositionC (Max)MnSiCrPSMoNi
 0.26-0.340.30-0.60≤0.401.80-2.20≤0.035≤0.350.30-0.501.80-2.20
Mechanical properties

 

Hardness(BHN)Impact strength(kg*m/cm2) 
≧4505.5